A comparative study of three glass ionomer base materials.

J. O. Burgess, N. Barghi, D. C. Chan, T. Hummert

Producción científica: Articlerevisión exhaustiva

32 Citas (Scopus)

Resumen

This study compared the compressive and diametral tensile strength, compressive modulus, shear bond strength to dentin and resin composite, marginal gap between the base and tooth in Class V cavity preparation, and fluoride release of three glass ionomer base materials. In general, visible light-cured (VLC) base materials outperform the autopolymerizing glass ionomer base Ketac-Bond. The compressive modulus is significantly less for the VLC glass ionomer materials Vitrebond and Fuji LC compared to Ketac-Bond. The Fuji LC had greater diametral tensile strength, compressive strength, bond to dentin and bond to resin composite than Vitrebond or Ketac-Bond. The fluoride release of Vitrebond was greater than Ketac-Bond or Fuji LC. The marginal gap at the tooth/base interface was significantly less with the Fuji LC compared to the other two materials.

Idioma originalEnglish (US)
Páginas (desde-hasta)137-141
Número de páginas5
PublicaciónAmerican journal of dentistry
Volumen6
N.º3
EstadoPublished - jun 1993

ASJC Scopus subject areas

  • General Dentistry

Huella

Profundice en los temas de investigación de 'A comparative study of three glass ionomer base materials.'. En conjunto forman una huella única.

Citar esto